Kool Mµ ® MAX: the next generation of sendust cores from Magnetics

For our new Kool Mµ MAX cores we supercharged our low core loss Kool Mµ material with 50% better DC bias performance for better power handling. Use of copper wire is minimized as Kool Mµ MAX maintains its inductance using less turns, resulting in savings in your overall component cost. With its super low losses, Kool Mu MAX does not mimic the temperature rise problems found in iron powder cores. Improve inductor efficiency at a fraction of the cost of High Flux with new Kool Mu MAX!

For more information on Magnetics' new Kool Mµ MAX
toroids, view our
technical bulletin.
Magnetics
 Material

Alloy Composition
DC Bias
Core Loss
Relative Cost
Saturation
Flux Density
Curie
 Temp.
60µ
µ flat to...
Kool Mµ MAX
FeSiAl
Better
Very Low
Medium
1.0T
500°C
900 kHz
Kool Mµ
FeSiAl
Good
Low
Lowest
1.0T
500°C
900 kHz
75 Series
FeSiAl
Better
Moderate
Low
1.5T
700°C
500 kHz
XFlux
FeSi
Best
High
Low
1.6T
700°C
500 kHz
High Flux
FeNi
Best
Moderate
High
1.5T
500°C
1 MHz
MPP
FeNiMo
Better
Very Low
Highest
0.8T
460°C
2 MHz